Original paper(Vol.49 No.11 pp.1242)

Deformation and Aging of Pd by Hydrogen Absorption-Desorption Cycles- Deformation@of Pd at a Hydrogen Absorption-Desorption Cycle-

Young-GUNG, Hideki SUEHIRO and Yuzuru SAKAI

Abstract:By using the electrolytic methodCthin plate Palladium specimens are loaded with hydrogen to examine the relation between the lattice expansion and the hydrogen absorption rateCand the relation between the lattice expansion and bulk deformation of specimens at each hydrogen absorbing rate on one hydrogen absorption-desorption cycle. The behavior of the lattice expansion on the hydrogen absorbing rate can be obtained by X-ray diffraction analyses. It is noted that the lattice size increases quickly with increasing hydrogen absorbing rate (H/Pd) up to 0.2Chowever, above the rate the lattice size keeps constant value. The expansion rate of the Pd plate specimen agree well with the lattice expansion rate in longitudinal and width direction of the specimens, though in thickness direction the expansion rate is about 5 times lager than other directions.

Key Words:Palladium, Electrochemical method, Hydrogen absorption, X-ray analysis, Lattice expansion